REXOLITE   1422     2000    2200

 

A BRIEF INTRODUCTION

 

 BACK  

       

ELECTRICAL PROPERTIES                                               PHYSICAL PROPERTIES

DIELECTRIC CONST. 2.53                                                              TENSILE STRENGTH 11,000 PSI

10 – 10,000 MC                                                                                    TENSILE MODULUS 4.5 x 105 PSI

DISSIPATION FACTOR                                                                     FLEXURAL STRENGTH 16,000 PSI

1MC              .00012                                                                              COMRESSIVE STRENGTH 33,000 PSI

10MC          .00025                                                                                FLEXURAL MODULUS 2 x 105 PSI

10,000MC  .00066                                                                                  IMPACT STRENGTH .3 FT. #/INCH

DIELECTRIC STRENGTH                                                                 SPECIFIC GRAVITY 1.05                                                                                                                                                 

STEP BY STEP                                                                                     COEFFICIENT OF LINEAR 7 x 10-5 / oC

1/32" THICK 1100 VOLTS / MIL                                                       THERMAL EXPANSION   

1/8 " THICK 500 VOLTS / MIL                                                          WATER ABSORPTION .05 %

SHORT TIME     

1/32" THICK 1200 VOLTS / MIL

1/8 " THICK 700 VOLTS / MIL

VOLUME RESISTIVITY 

1016 OHM-CM

SURFACE RESISTIVITY

1014 OHMS

 

 